Solid content: 14 (+1) %
Viscosity (mpa.s): 3.5~4.0 mPa.s
color system: Blue
exposure latent image: color reduction
Photosensitive wavelength: 405~410nm UVlaser
Exposure energy: 35~45mW
Development temperature:23+2°C
developing time:20+5Secs
resolution:2~98%at 200Ipi
Durability:50,000 impressions for unbaked version, 150,000 impressions for baked version (running capacity varies with printing conditions)
Storage conditions and period:Avoid light, ≤25°C, dry, one year
Hot Tags: positive coating ctcp photosensitive liquid, China positive coating ctcp photosensitive liquid manufacturers, factory, 3 5 Ditert butylbenzoic acid, 4 5 Dimethyl 3 hydroxy 2 5 dihydrofuran 2 one, 2 2 AZOBIS 2 2 IMIDAZOLIN 2 YL PROPANE DIHYDROCHLORIDE, Phenylmethyl silicone oil, Benzalkonium Chloride, Tetramethylol acetylenediurea